Wood Chips

The forests are our own, and we produce wood chips for cellulose and biomass using specific equipment with organized logistics in ports of Santa Catarina and Rio Grande do Sul.

Wood chips have a variety of applications and are frequently used as raw material in various industries. This production process involves the transformation of biological assets in their entirety, harnessing 100% of their potential. We believe it is our responsibility to ensure the sustainability of the products we deliver, and therefore, we can provide the required certificates to meet export demands.

This broad spectrum of uses for these assets worldwide qualifies us to export logs in various diameters and lengths, with JAS volume measurement, as well as processed wood for specific applications in the timber industry.

Sugar imageSugar imageSugar imageSugar imageSugar imageSugar imageSugar imageSugar imageSugar image

Specifications for Eucalyptus Chips

Over-thicked chips percentage< 20%
Width (maximum size)30mm
Width (minimum size)15mm
Thickness (average)2 to 8 mm
ShapeToothpick Shape
Age of Pinus trees8 to 35 years
Age of Eucalyptus trees> 18 years
Density (average)330 - 550 Kg/m³
Moisture of stocked chips36% to 39%
Lower Calorific Power2580 Kcal/Kg
Upper CalorificPower3776 Kcal/Kg
Dry Calorific Power4400 Kcal/Kg
Ash content26% to 30%
Carbon Dry Basis48%
Carbon Natural Basis15%/m³/year
Chlorine0.01 - 0.9%
Impurities percentageTo be determined with future tests
Soluble and insoluble LigninSoluble: 2.7% - Insoluble: 25.5%

Specifications for Pine Chips

Over-thicked chips percentage< 20%
Width (maximum size)30mm
Width (minimum size)15mm
Thickness (average)2 to 8 mm
ShapeToothpick Shape
Age of Pinus trees8 to 35 years
Density (average)420 - 500 Kg/m³
Moisture of stocked chips36% to 39%
Lower Calorific Power2700 Kcal/Kg
Upper CalorificPower4276 Kcal/Kg
Dry Calorific Power4900 Kcal/Kg
Ash content26% to 30%
Carbon Dry Basis48%
Carbon Natural Basis15%/m³/year
ChlorineDoes not require fertilization
Impurities percentageTo be determined with future tests
Soluble and insoluble LigninSoluble: 0.9% - Insoluble: 30.20%